A self-adhesive improved asphalt sheet with excellent heat resistance, cold resistance, drug resistance, and durability around fiber reinforcement with high tensile and training performance, and a self-adhesive method with rubberized asphalt gel combined at the bottom
Scope of Application
Packaging Unit
|
Item | Performance Standard | |||
---|---|---|---|---|
Classification according to use | Non-exposure multiple layer waterproof | |||
Classification according to material composition | TYPE A | |||
Tensile Performance | Tensile Strength (N/㎜) | Untreated | Above 5.0 | |
After heating | Above 80% of untreated test value | |||
After soaking alkali | ||||
Coefficient of Expansion (%) | Untreated | Above 15 | ||
After heating | Above 80% of untreated test value | |||
After soaking alkali | ||||
Tensile Product (N·%/㎜) | Untreated | Above 200 | ||
Tearing Performance (N) | Above 20 | |||
Heat Resistance Performance | Roll Down Length (㎜) | Below 5 | ||
Appearance | Will not roll down or shoot out. | |||
Fatigue Performance | Will not rip, crack, or be blocked | |||
Dimensional stability | Change Rate of value (%) | 0.0±1.0 |
||
Appearance | No creases, bending, or detachment between layers | |||
Joint Performance (N/㎜) | Above 5.0 or above 70% of untreated tensile strength | |||
Pitting Performance | No hole |